20oz Skinny Tumbler Sublimation: Clean Wraps Without Ghosting

Direct Answer:

Print mirrored, dry, and shrink sleeve tight. Oven at 375–400°F for 4–6 minutes, rotate halfway. Cool upright. Ghosting = slack or movement.

Steps

  1. Mirror print and dry for 10 minutes so print is dry.
  2. Clean tumbler with 70% Rubbing Alcohol.
  3. Wrap tight and tape seam full height.
  4. Shrink sleeve until smooth.
  5. Bake at 375–400°F: 2–3 min, rotate 180°, 2–3 min more.
  6. Cool upright to vent steam.

Specs

Variable Value
Oven Convection preferred
Temp 375–400°F
Total Time 4–6 minutes
Sleeve Shrink fully, no wrinkles
Seam Straight, no overlap

Risks

  • Gap at seam = paper too short → butt edges precisely.
  • Tiger stripes = airflow issue → rotate halfway.
  • Brown edges = overcook → trim paper, shorten time.

FAQs

Press vs oven? Oven is more forgiving for wraps.

Why brown edges? Overcooked — cut paper shorter or reduce time.

Sources

Coating vendor specs and Pressing Images oven profiles.